TaeguTec Platter CCGT09T304 FL, K10

AVN varenr.: CCGT09T304FLK10
Artikel nummer: CCGT09T304FLK10

Beskrivelse

Cutting Speed for: CCGT FL K10 
ISO Material Material Description Material Condition Cutting Speed Recommendations
K 15 Grey cast iron (GG) Pearlitic/ferritic :180 110-180 m/min
K 16 Grey cast iron (GG) Pearlitic/martensiti :260 95-140 m/min
K 17 Nodular cast iron (GGG) Ferritic :160 95-135 m/min
K 18 Nodular cast iron (GGG) Pearlitic :250 90-125 m/min
K 19 Malleable cast iron. Ferritic :130 110-140 m/min
K 20 Malleable cast iron. Pearlitic :230 90-125 m/min
N 21 Aluminum-wrought alloy. Not cureable : 60 200-1000 m/min
N 22 Aluminum-wrought alloy. Cured :100 200-1000 m/min
N 23 Aluminum-cast, alloyed <12% Si. Not cureable : 75 50-400 m/min
N 24 Aluminum-cast, alloyed. Cured : 90 50-500 m/min
N 25 Aluminum-cast, alloyed >12% Si. High temperature :130 40-350 m/min
N 26 Copper alloys >1% pb. Free cutting :110 50-500 m/min
N 27 Copper alloys. Brass : 90 50-500 m/min
N 28 Copper alloys. Electrolitic copper :100 30-300 m/min
N 29 Non metallic. Duro& fiber plastics : 60 50-300 m/min
N 30 Non metallic Hard rubber : 55 50-150 m/min
S 31 High temp. alloys Fe based. Annealed :200 55-85 m/min
S 32 High temp. alloys Fe based. Cured :280 40-65 m/min
S 33 High temp. alloys. Ni or Co based. Annealed :250 32-55 m/min
S 34 High temp. alloys. Ni or Co based. Cured :350 21-40 m/min
S 35 High temp. alloys. Ni or Co based. Castr :320 16-26 m/min
S 36 Titanium Ti alloys. :310 50-75 m/min
S 37 Titanium Ti alloys. Alpha+beta alloys cu :310 45-70 m/min

Relaterede produkter